One thing we love at London Jewellery School is an opportunity to try out new tools and materials, so when our friends at Shesto, who produce the JewelTool range, offered the change to try out a new moulding compound we were quick to accept.

ComposiMold is a reusable moulding medium that you can melt in the microwave so we set Bronagh Miskelly, who regularly works with resin, the task of trying it out.

I have tried out reusable moulding compound before and found it fiddly requiring a sugar thermometer and a certain amount of heating and cooling before it was at the right temperature to pour. I also had trouble with achieving a smooth surface on the mould. So I was interested to try a something that claimed to be easier.

resin jewellery making

I used ComposiMold Firm which looks like a brown jelly in a tub. Melting is very simple – you work in 30 second bursts and stir the “jelly” between bursts. It only took a couple of minutes for it all to be melted and there was no mess.

resin jewellery making

I’d put the tub on an old pyrex dish to be on the safe side and even though I’d no problems I’d recommend that because I was able to rest my stirrer on it and catch any drips.

resin jewellery making

The instructions recommend using heat proof materials to contain your moulds. I used dishes from microwave meals (you can usually collect these after lunch at LJS) and coated the surface and the items I was using as blanks with petroleum jelly. Once the compound was liquid it was just a case of pouring it gently in to the moulds – I poured too quickly at first and got bubbles which I had to try to tap out, but got it smoother for the rings.

Then it was a case of letting it cool and set.

resin jewellery making

As an experiment I placed the ring blanks the same wide tray and then cut the mould down return the excess to the ComposiMold tub along with any set drips etc.

mold 8

I also tested my finished moulds with resin. I found that you do need to use a thin costing of petroleum jelly of other release agent. I tested on ring with and one without. I couldn’t get the cast ring out of the uncoated mould but I was able to cut away the mould and then remelt the material and make a new one.

The moulds worked well. The rings only required a small amount of sanding so I was generally pleased with the outcome.

resin jewellery

I haven’t done enough to tell how long one of these moulds will last or if they will tear. But I have tested reusing the compound and found it quick and easy to make more moulds. On the whole I was impressed by the ease of use and initial results.

We hope to stock ComposiMold in the LJS pop-up shop very soon.

 

One Comment

  1. Posted March 22, 2015 at 11:04 pm | Permalink | Reply

    Please could you let us know which photo gallery you are referring to?

    Thanks you

Leave a Reply

Fill in your details below or click an icon to log in:

WordPress.com Logo

You are commenting using your WordPress.com account. Log Out / Change )

Twitter picture

You are commenting using your Twitter account. Log Out / Change )

Facebook photo

You are commenting using your Facebook account. Log Out / Change )

Google+ photo

You are commenting using your Google+ account. Log Out / Change )

Connecting to %s

%d bloggers like this: